Operation
In most of its applications, gas metal arc welding is a fairly simple welding process to learn, requiring no more than several days to master basic welding technique. Even when welding is performed by well-trained operators, however, weld quality can fluctuate, since it depends on a number of external factors. And all GMAW is dangerous, though perhaps less so than some other welding methods, such as shielded metal arc welding.
Friday, December 22, 2006
Technique
Technique
The basic technique for GMAW is quite simple, since the electrode is fed automatically through the torch. In gas tungsten arc welding, the welder must handle a welding torch in one hand and a separate filler wire in the other, and in shielded metal arc welding, the operator must frequently chip off slag and change welding electrodes. GMAW, on the other hand, requires only that the operator guide the welding gun with proper position and orientation along the area being welded. Keeping a consistent contact tip-to-work distance (the stickout distance) is important, because a long stickout distance can cause the electrode to overheat and will also waste shielding gas. The orientation of the gun is also important it should be held so as to bisect the angle between the workpieces; that is, at 45 degrees for a fillet weld and 90 degrees for welding a flat surface. The travel angle or lead angle is the angle of the torch with respect to the direction of travel, and it should generally remain approximately vertical. However, the desirable angle changes somewhat depending on the type of shielding gas used with pure inert gases, the bottom of the torch is out often slightly in front of the upper section, while the opposite is true when the welding atmosphere is carbon dioxide.
The basic technique for GMAW is quite simple, since the electrode is fed automatically through the torch. In gas tungsten arc welding, the welder must handle a welding torch in one hand and a separate filler wire in the other, and in shielded metal arc welding, the operator must frequently chip off slag and change welding electrodes. GMAW, on the other hand, requires only that the operator guide the welding gun with proper position and orientation along the area being welded. Keeping a consistent contact tip-to-work distance (the stickout distance) is important, because a long stickout distance can cause the electrode to overheat and will also waste shielding gas. The orientation of the gun is also important it should be held so as to bisect the angle between the workpieces; that is, at 45 degrees for a fillet weld and 90 degrees for welding a flat surface. The travel angle or lead angle is the angle of the torch with respect to the direction of travel, and it should generally remain approximately vertical. However, the desirable angle changes somewhat depending on the type of shielding gas used with pure inert gases, the bottom of the torch is out often slightly in front of the upper section, while the opposite is true when the welding atmosphere is carbon dioxide.
Quality
Quality
Two of the most prevalent quality problems in GMAW are dross and porosity. If not controlled, they can lead to weaker, less ductile welds. Dross is an especially common problem in aluminum GMAW welds, normally coming from particles of aluminum oxide or aluminum nitride present in the electrode or base materials. Electrodes and workpieces must be brushed with a wire brush or chemically treated to remove oxides on the surface. Any oxygen in contact with the weld pool, whether from the atmosphere or the shielding gas, causes dross as well. As a result, sufficient flow of inert shielding gases is necessary, and welding in volatile air should be avoided.
In GMAW the primary cause of porosity is gas entrapment in the weld pool, which occurs when the metal solidifies before the gas escapes. The gas can come from impurities in the shielding gas or on the workpiece, as well as from an excessively long or violent arc. Generally, the amount of gas entrapped is directly related to the cooling rate of the weld pool. Because of its higher thermal conductivity, aluminum welds are especially susceptible to greater cooling rates and thus additional porosity. To reduce it, the workpiece and electrode should be clean, the welding speed diminished and the current set high enough to provide sufficient heat input and stable metal transfer but low enough that the arc remains steady. Preheating can also help reduce the cooling rate in some cases by reducing the temperature gradient between the weld area and the base material.
Two of the most prevalent quality problems in GMAW are dross and porosity. If not controlled, they can lead to weaker, less ductile welds. Dross is an especially common problem in aluminum GMAW welds, normally coming from particles of aluminum oxide or aluminum nitride present in the electrode or base materials. Electrodes and workpieces must be brushed with a wire brush or chemically treated to remove oxides on the surface. Any oxygen in contact with the weld pool, whether from the atmosphere or the shielding gas, causes dross as well. As a result, sufficient flow of inert shielding gases is necessary, and welding in volatile air should be avoided.
In GMAW the primary cause of porosity is gas entrapment in the weld pool, which occurs when the metal solidifies before the gas escapes. The gas can come from impurities in the shielding gas or on the workpiece, as well as from an excessively long or violent arc. Generally, the amount of gas entrapped is directly related to the cooling rate of the weld pool. Because of its higher thermal conductivity, aluminum welds are especially susceptible to greater cooling rates and thus additional porosity. To reduce it, the workpiece and electrode should be clean, the welding speed diminished and the current set high enough to provide sufficient heat input and stable metal transfer but low enough that the arc remains steady. Preheating can also help reduce the cooling rate in some cases by reducing the temperature gradient between the weld area and the base material.
Safety
Safety
Gas metal arc welding can be dangerous if proper precautions are not taken. Since GMAW employs an electric arc, welders wear protective clothing, including heavy leather gloves and protective long sleeve jackets, to avoid exposure to extreme heat and flames. In addition, the brightness of the electric arc can cause arc eye, in which ultraviolet light causes the inflammation of the cornea and can burn the retinas of the eyes. Helmets with dark face plates are worn to prevent this exposure, and in recent years, new helmet models have been produced that feature a liquid crystal-type face plate that self-darkens upon exposure to high amounts of UV light. Transparent welding curtains, made of a polyvinyl chloride plastic film, are often used to shield nearby workers and bystanders from exposure to the UV light from the electric arc.
Welders are also often exposed to dangerous gases and particulate matter. GMAW produces smoke containing particles of various types of oxides, and the size of the particles in question tends to influence the toxicity of the fumes, with smaller particles presenting a greater danger. Additionally, carbon dioxide and ozone gases can prove dangerous if ventilation is inadequate. Furthermore, because the use of compressed gases in GMAW pose an explosion and fire risk, some common precautions include limiting the amount of oxygen in the air and keeping combustible materials away from the workplace.
Gas metal arc welding can be dangerous if proper precautions are not taken. Since GMAW employs an electric arc, welders wear protective clothing, including heavy leather gloves and protective long sleeve jackets, to avoid exposure to extreme heat and flames. In addition, the brightness of the electric arc can cause arc eye, in which ultraviolet light causes the inflammation of the cornea and can burn the retinas of the eyes. Helmets with dark face plates are worn to prevent this exposure, and in recent years, new helmet models have been produced that feature a liquid crystal-type face plate that self-darkens upon exposure to high amounts of UV light. Transparent welding curtains, made of a polyvinyl chloride plastic film, are often used to shield nearby workers and bystanders from exposure to the UV light from the electric arc.
Welders are also often exposed to dangerous gases and particulate matter. GMAW produces smoke containing particles of various types of oxides, and the size of the particles in question tends to influence the toxicity of the fumes, with smaller particles presenting a greater danger. Additionally, carbon dioxide and ozone gases can prove dangerous if ventilation is inadequate. Furthermore, because the use of compressed gases in GMAW pose an explosion and fire risk, some common precautions include limiting the amount of oxygen in the air and keeping combustible materials away from the workplace.
Globular
Globular
GMAW with globular metal transfer is often considered the most undesirable of the four major GMAW variations, because of its tendency to produce high heat, a poor weld surface, and spatter. The method was originally developed as a cost efficient way to weld steel using GMAW, because this variation uses carbon dioxide, a less expensive shielding gas than argon. Adding to its economic advantage was its high deposition rate, allowing welding speeds of up to 110 mm/s (250 in/min). As the weld is made, a ball of molten metal from the electrode tends to build up on the end of the electrode, often in irregular shapes with a larger diameter than the electrode itself. When the droplet finally detaches either by gravity or short circuiting, it falls to the workpiece, leaving an uneven surface and often causing spatter. As a result of the large molten droplet, the process is generally limited to flat and horizontal welding positions. The high amount of heat generated also is a downside, because it forces the welder to use a larger electrode wire, increases the size of the weld pool, and causes greater residual stresses and distortion in the weld area.
GMAW with globular metal transfer is often considered the most undesirable of the four major GMAW variations, because of its tendency to produce high heat, a poor weld surface, and spatter. The method was originally developed as a cost efficient way to weld steel using GMAW, because this variation uses carbon dioxide, a less expensive shielding gas than argon. Adding to its economic advantage was its high deposition rate, allowing welding speeds of up to 110 mm/s (250 in/min). As the weld is made, a ball of molten metal from the electrode tends to build up on the end of the electrode, often in irregular shapes with a larger diameter than the electrode itself. When the droplet finally detaches either by gravity or short circuiting, it falls to the workpiece, leaving an uneven surface and often causing spatter. As a result of the large molten droplet, the process is generally limited to flat and horizontal welding positions. The high amount of heat generated also is a downside, because it forces the welder to use a larger electrode wire, increases the size of the weld pool, and causes greater residual stresses and distortion in the weld area.
Short-circuiting
Short-circuiting
Further developments in welding steel with GMAW led to a variation known as short-circuiting or short-arc GMAW, in which carbon dioxide shields the weld, the electrode wire is smaller, and the current is lower than for the globular method. As a result of the lower current, the heat input for the short-arc variation is reduced, making it possible to weld thinner materials while decreasing the amount of distortion and residual stress in the weld area. As in globular welding, molten droplets form on the tip of the electrode, but instead of dropping to the weld pool, they bridge the gap between the electrode and the weld pool as a result of the greater wire feed rate. This causes a short circuit and extinguishes the arc, but it is quickly reignited after the surface tension of the weld pool pulls the molten metal bead off the electrode tip. This process is repeated about 100 times per second, making the arc appear constant to the human eye. This type of metal transfer provides better weld quality and less spatter than the globular variation, and it allows for welding in all positions, but generally the process is much slower than globular GMAW. Another difficulty is maintaining a stable arc, because it depends on achieving a consistent and high short-circuiting frequency, which can only be accomplished with a good power source, suitable welding conditions, and significant welder skill. Like the globular variation, it can only be used on ferrous metals.
Further developments in welding steel with GMAW led to a variation known as short-circuiting or short-arc GMAW, in which carbon dioxide shields the weld, the electrode wire is smaller, and the current is lower than for the globular method. As a result of the lower current, the heat input for the short-arc variation is reduced, making it possible to weld thinner materials while decreasing the amount of distortion and residual stress in the weld area. As in globular welding, molten droplets form on the tip of the electrode, but instead of dropping to the weld pool, they bridge the gap between the electrode and the weld pool as a result of the greater wire feed rate. This causes a short circuit and extinguishes the arc, but it is quickly reignited after the surface tension of the weld pool pulls the molten metal bead off the electrode tip. This process is repeated about 100 times per second, making the arc appear constant to the human eye. This type of metal transfer provides better weld quality and less spatter than the globular variation, and it allows for welding in all positions, but generally the process is much slower than globular GMAW. Another difficulty is maintaining a stable arc, because it depends on achieving a consistent and high short-circuiting frequency, which can only be accomplished with a good power source, suitable welding conditions, and significant welder skill. Like the globular variation, it can only be used on ferrous metals.
Spray
Spray
Spray transfer GMAW was the first metal transfer method used in GMAW, best suited for welding aluminum and stainless steel while employing an inert shielding gas and a relatively thick electrode. In this variation, molten metal droplets (with diameters smaller than the electrode diameter) are rapidly passed along the stable electric arc from the electrode to the workpiece, essentially eliminating spatter and resulting in a high-quality weld finish. However, high amounts of voltage and current are necessary, which means that the process involves high heat input and a large weld area and heat-affected zone. As a result, it is generally used only on workpieces of thicknesses above about 6 mm (0.25 in). Because of the large weld pool, it is often limited to flat and horizontal welding positions, but when a smaller electrode is used in conjunction with lower heat input, its versatility increases. The maximum deposition rate for spray arc GMAW is relatively high; about 60 mm/s (150 in/min).
Spray transfer GMAW was the first metal transfer method used in GMAW, best suited for welding aluminum and stainless steel while employing an inert shielding gas and a relatively thick electrode. In this variation, molten metal droplets (with diameters smaller than the electrode diameter) are rapidly passed along the stable electric arc from the electrode to the workpiece, essentially eliminating spatter and resulting in a high-quality weld finish. However, high amounts of voltage and current are necessary, which means that the process involves high heat input and a large weld area and heat-affected zone. As a result, it is generally used only on workpieces of thicknesses above about 6 mm (0.25 in). Because of the large weld pool, it is often limited to flat and horizontal welding positions, but when a smaller electrode is used in conjunction with lower heat input, its versatility increases. The maximum deposition rate for spray arc GMAW is relatively high; about 60 mm/s (150 in/min).